TURBINE PART MADE OF SUPERALLOY COMPRISING RHENIUM AND/OR RUTHENIUM AND ASSOCIATED MANUFACTURING METHOD
Extensive patent search conducted by a registered patent agent
Patent search done by experts in under 48hrs
₹999
₹399
Abstract
Information
Inventors
Applicants
Specification
Documents
PCT NATIONAL PHASE APPLICATION
Published
Filed on 31 March 2020
Patent Information
| Application ID | 202017014461 |
| Date of Application | 31/03/2020 |
Documents
| Name | Date |
|---|---|
| 202017014461-IntimationOfGrant27-12-2023.pdf | 27/12/2023 |
| 202017014461-PatentCertificate27-12-2023.pdf | 27/12/2023 |
| 202017014461-FORM 3 [14-06-2023(online)].pdf | 14/06/2023 |
| 202017014461-CLAIMS [20-10-2022(online)].pdf | 20/10/2022 |
| 202017014461-FER_SER_REPLY [20-10-2022(online)].pdf | 20/10/2022 |
| 202017014461-Information under section 8(2) [18-10-2022(online)].pdf | 18/10/2022 |
| 202017014461-FORM 3 [13-07-2022(online)].pdf | 13/07/2022 |
| 202017014461-FER.pdf | 25/04/2022 |
| 202017014461.pdf | 19/10/2021 |
| 202017014461-FORM 3 [15-09-2021(online)].pdf | 15/09/2021 |
| 202017014461-FORM 18 [25-08-2021(online)].pdf | 25/08/2021 |
| 202017014461-FORM 3 [23-09-2020(online)].pdf | 23/09/2020 |
| 202017014461-Proof of Right [23-09-2020(online)].pdf | 23/09/2020 |
| 202017014461-FORM-26 [25-05-2020(online)].pdf | 25/05/2020 |
| 202017014461-certified copy of translation [29-04-2020(online)].pdf | 29/04/2020 |
| 202017014461-COMPLETE SPECIFICATION [31-03-2020(online)].pdf | 31/03/2020 |
| 202017014461-DECLARATION OF INVENTORSHIP (FORM 5) [31-03-2020(online)].pdf | 31/03/2020 |
| 202017014461-DRAWINGS [31-03-2020(online)].pdf | 31/03/2020 |
| 202017014461-FORM 1 [31-03-2020(online)].pdf | 31/03/2020 |
| 202017014461-NOTIFICATION OF INT. APPLN. NO. & FILING DATE (PCT-RO-105) [31-03-2020(online)].pdf | 31/03/2020 |
| 202017014461-STATEMENT OF UNDERTAKING (FORM 3) [31-03-2020(online)].pdf | 31/03/2020 |
| 202017014461-TRANSLATIOIN OF PRIOIRTY DOCUMENTS ETC. [31-03-2020(online)].pdf | 31/03/2020 |
Refer a friend