PRE WELD HEAT TREATMENT FOR A NICKEL BASED SUPERALLOY
Extensive patent search conducted by a registered patent agent
Patent search done by experts in under 48hrs
₹999
₹399
Abstract
Information
Inventors
Applicants
Specification
Documents
PCT NATIONAL PHASE APPLICATION
Published
Filed on 28 July 2015
Patent Information
| Application ID | 6615/DELNP/2015 |
| Date of Application | 28/07/2015 |
Documents
| Name | Date |
|---|---|
| 6615-DELNP-2015-IntimationOfGrant01-12-2022.pdf | 01/12/2022 |
| 6615-DELNP-2015-PatentCertificate01-12-2022.pdf | 01/12/2022 |
| 6615-DELNP-2015-Correspondence-041119.pdf | 06/11/2019 |
| 6615-DELNP-2015-Power of Attorney-041119.pdf | 06/11/2019 |
| 6615-DELNP-2015-CLAIMS [24-10-2019(online)].pdf | 24/10/2019 |
| 6615-DELNP-2015-COMPLETE SPECIFICATION [24-10-2019(online)].pdf | 24/10/2019 |
| 6615-DELNP-2015-DRAWING [24-10-2019(online)].pdf | 24/10/2019 |
| 6615-DELNP-2015-FER_SER_REPLY [24-10-2019(online)].pdf | 24/10/2019 |
| 6615-DELNP-2015-FORM-26 [24-10-2019(online)].pdf | 24/10/2019 |
| 6615-DELNP-2015-Information under section 8(2) (MANDATORY) [24-10-2019(online)].pdf | 24/10/2019 |
| 6615-DELNP-2015-OTHERS [24-10-2019(online)].pdf | 24/10/2019 |
| 6615-DELNP-2015-PETITION UNDER RULE 137 [24-10-2019(online)].pdf | 24/10/2019 |
| 6615-DELNP-2015-FORM 3 [02-07-2019(online)].pdf | 02/07/2019 |
| 6615-DELNP-2015-FER.pdf | 25/04/2019 |
| 6615-delnp-2015-Assignment-(21-08-2015).pdf | 21/08/2015 |
| 6615-delnp-2015-Correspondence Others-(21-08-2015).pdf | 21/08/2015 |
| 6615-DELNP-2015.pdf | 31/07/2015 |
| Description(Complete) [28-07-2015(online)].pdf | 28/07/2015 |
| Form 1 [28-07-2015(online)].pdf | 28/07/2015 |
| Form 3 [28-07-2015(online)].pdf | 28/07/2015 |
| Form 5 [28-07-2015(online)].pdf | 28/07/2015 |
| Power of Attorney [28-07-2015(online)].pdf | 28/07/2015 |
| Priority Document [28-07-2015(online)].pdf | 28/07/2015 |
Refer a friend