METHOD AND SYSTEM FOR FAST CHARGING WITH MINIMUM CAPACITY FADE

Patent Search in India

  • tick

    Extensive patent search conducted by a registered patent agent

  • tick

    Patent search done by experts in under 48hrs

₹999

₹399

Talk to expert

METHOD AND SYSTEM FOR FAST CHARGING WITH MINIMUM CAPACITY FADE

ORDINARY APPLICATION

Published

date

Filed on 9 October 2020

Patent Information

Application ID202041044102
Date of Application09/10/2020

Documents

NameDate
202041044102-IntimationOfGrant14-12-2023.pdf14/12/2023
202041044102-PatentCertificate14-12-2023.pdf14/12/2023
202041044102-Written submissions and relevant documents [02-11-2023(online)].pdf02/11/2023
202041044102-Correspondence to notify the Controller [16-10-2023(online)].pdf16/10/2023
202041044102-FORM-26 [16-10-2023(online)].pdf16/10/2023
202041044102-US(14)-HearingNotice-(HearingDate-19-10-2023).pdf19/09/2023
202041044102-8(i)-Substitution-Change Of Applicant - Form 6 [15-04-2023(online)].pdf15/04/2023
202041044102-ASSIGNMENT DOCUMENTS [15-04-2023(online)].pdf15/04/2023
202041044102-PA [15-04-2023(online)].pdf15/04/2023
202041044102-CLAIMS [29-11-2022(online)].pdf29/11/2022
202041044102-CORRESPONDENCE [29-11-2022(online)].pdf29/11/2022
202041044102-DRAWING [29-11-2022(online)].pdf29/11/2022
202041044102-FER_SER_REPLY [29-11-2022(online)].pdf29/11/2022
202041044102-OTHERS [29-11-2022(online)].pdf29/11/2022
202041044102-FER.pdf13/06/2022
202041044102-Correspondence_Form 1_15-11-2021.pdf15/11/2021
202041044102-COMPLETE SPECIFICATION [09-10-2020(online)].pdf09/10/2020
202041044102-DECLARATION OF INVENTORSHIP (FORM 5) [09-10-2020(online)].pdf09/10/2020
202041044102-DRAWINGS [09-10-2020(online)].pdf09/10/2020
202041044102-FORM 1 [09-10-2020(online)].pdf09/10/2020
202041044102-FORM 18 [09-10-2020(online)].pdf09/10/2020
202041044102-POWER OF AUTHORITY [09-10-2020(online)].pdf09/10/2020
202041044102-PROOF OF RIGHT [09-10-2020(online)].pdf09/10/2020
202041044102-REQUEST FOR EXAMINATION (FORM-18) [09-10-2020(online)].pdf09/10/2020
202041044102-STATEMENT OF UNDERTAKING (FORM 3) [09-10-2020(online)].pdf09/10/2020
earn

Refer a friend