METHOD FOR POST-BUILT HEAT TREATMENT OF ADDITIVELY MANUFACTURED COMPONENETS MADE OF GAMMA-PRIME STRENGTHENED SUPERALLOYS
Extensive patent search conducted by a registered patent agent
Patent search done by experts in under 48hrs
₹999
₹399
Abstract
Information
Inventors
Applicants
Specification
Documents
CONVENTIONAL APPLICATION
Published
Filed on 30 April 2015
Patent Information
| Application ID | 1207/DEL/2015 |
| Date of Application | 30/04/2015 |
Documents
| Name | Date |
|---|---|
| 1207-DEL-2015-FER.pdf | 17/10/2021 |
| 1207-DEL-2015-FORM 18 [20-04-2018(online)]-1.pdf | 20/04/2018 |
| 1207-DEL-2015-FORM 18 [20-04-2018(online)].pdf | 20/04/2018 |
| 1207-DEL-2015-FORM 3 [09-01-2018(online)].pdf | 09/01/2018 |
| Assignment [15-04-2017(online)].pdf | 15/04/2017 |
| Form 6 [15-04-2017(online)].pdf | 15/04/2017 |
| Power of Attorney [15-04-2017(online)].pdf | 15/04/2017 |
| 1207-del-2015-Correspondence-090117.pdf | 23/01/2017 |
| 1207-del-2015-GPA-090117.pdf | 23/01/2017 |
| 1207-del-2015-Others-090117.pdf | 23/01/2017 |
| Form 13 [18-11-2016(online)].pdf | 18/11/2016 |
| Other Document [18-11-2016(online)].pdf | 18/11/2016 |
| Form 13 [10-11-2016(online)].pdf | 10/11/2016 |
| Other Document [10-11-2016(online)].pdf | 10/11/2016 |
| 1207-del-2015-Correspondence Others-(04-09-2015).pdf | 04/09/2015 |
| 1207-del-2015-Form-3-(04-09-2015).pdf | 04/09/2015 |
| 1207-del-2015-Correspodence Others-(12-08-2015).pdf | 12/08/2015 |
| 1207-del-2015-Form-1-(12-08-2015).pdf | 12/08/2015 |
| 1207-del-2015-Others-(12-08-2015).pdf | 12/08/2015 |
| 1207-del-2015-Abstract-(30-04-2015).pdf | 30/04/2015 |
| 1207-del-2015-Claims-(30-04-2015).pdf | 30/04/2015 |
| 1207-del-2015-Correspondence Others-(30-04-2015).pdf | 30/04/2015 |
| 1207-del-2015-Description (Complete)-(30-04-2015).pdf | 30/04/2015 |
| 1207-del-2015-Drawings-(30-04-2015).pdf | 30/04/2015 |
| 1207-del-2015-Form-1-(30-04-2015).pdf | 30/04/2015 |
| 1207-del-2015-Form-2-(30-04-2015).pdf | 30/04/2015 |
| 1207-del-2015-Form-3-(30-04-2015).pdf | 30/04/2015 |
| 1207-del-2015-Form-5-(30-04-2015).pdf | 30/04/2015 |
| 1207-del-2015-GPA-(30-04-2015).pdf | 30/04/2015 |
Refer a friend