LOW DENSITY NICKEL-BASED SUPERALLOY HAVING HIGH MECHANICAL STRENGTH AND ENVIRONMENTAL ROBUSTNESS AT A HIGH TEMPERATURE

Patent Search in India

  • tick

    Extensive patent search conducted by a registered patent agent

  • tick

    Patent search done by experts in under 48hrs

₹999

₹399

Talk to expert

LOW DENSITY NICKEL-BASED SUPERALLOY HAVING HIGH MECHANICAL STRENGTH AND ENVIRONMENTAL ROBUSTNESS AT A HIGH TEMPERATURE

PCT NATIONAL PHASE APPLICATION

Published

date

Filed on 13 July 2021

Patent Information

Application ID202117031384
Date of Application13/07/2021

Documents

NameDate
202117031384-ABSTRACT [25-05-2023(online)].pdf25/05/2023
202117031384-CLAIMS [25-05-2023(online)].pdf25/05/2023
202117031384-COMPLETE SPECIFICATION [25-05-2023(online)].pdf25/05/2023
202117031384-FER_SER_REPLY [25-05-2023(online)].pdf25/05/2023
202117031384-FORM 3 [25-05-2023(online)].pdf25/05/2023
202117031384-Information under section 8(2) [25-05-2023(online)].pdf25/05/2023
202117031384-FER.pdf03/01/2023
202117031384-FORM 18 [26-12-2022(online)].pdf26/12/2022
202117031384.pdf19/10/2021
202117031384-FORM 3 [08-10-2021(online)].pdf08/10/2021
202117031384-FORM-26 [08-10-2021(online)].pdf08/10/2021
202117031384-FORM-26 [10-08-2021(online)].pdf10/08/2021
202117031384-COMPLETE SPECIFICATION [13-07-2021(online)].pdf13/07/2021
202117031384-DECLARATION OF INVENTORSHIP (FORM 5) [13-07-2021(online)].pdf13/07/2021
202117031384-FORM 1 [13-07-2021(online)].pdf13/07/2021
202117031384-PRIORITY DOCUMENTS [13-07-2021(online)].pdf13/07/2021
202117031384-PROOF OF RIGHT [13-07-2021(online)].pdf13/07/2021
202117031384-STATEMENT OF UNDERTAKING (FORM 3) [13-07-2021(online)].pdf13/07/2021
earn

Refer a friend