"NEW INVENTION OF LOW COST CREEP TESTING MACHINE WITH VARIABLE TEMPERATURE AND ENVIRONMENTAL AND ENVIRONMENTAL CONDITIONS FOR COMPOSITE MATERIAL(PMMC)
Extensive patent search conducted by a registered patent agent
Patent search done by experts in under 48hrs
₹999
₹399
Abstract
Information
Inventors
Applicants
Specification
Documents
ORDINARY APPLICATION
Published
Filed on 26 December 2017
Patent Information
| Application ID | 201741046532 |
| Date of Application | 26/12/2017 |
Documents
| Name | Date |
|---|---|
| 201741046532-IntimationOfGrant30-01-2024.pdf | 30/01/2024 |
| 201741046532-PatentCertificate30-01-2024.pdf | 30/01/2024 |
| 201741046532-Annexure [16-01-2024(online)].pdf | 16/01/2024 |
| 201741046532-FORM 13 [16-01-2024(online)].pdf | 16/01/2024 |
| 201741046532-RELEVANT DOCUMENTS [16-01-2024(online)].pdf | 16/01/2024 |
| 201741046532-Written submissions and relevant documents [16-01-2024(online)].pdf | 16/01/2024 |
| 201741046532-Correspondence to notify the Controller [07-12-2023(online)].pdf | 07/12/2023 |
| 201741046532-Correspondence to notify the Controller [05-12-2023(online)].pdf | 05/12/2023 |
| 201741046532-US(14)-HearingNotice-(HearingDate-02-01-2024).pdf | 04/12/2023 |
| 201741046532-FER.pdf | 17/10/2021 |
| 201741046532-FORM 13 [15-07-2021(online)].pdf | 15/07/2021 |
| 201741046532-FORM-26 [15-07-2021(online)].pdf | 15/07/2021 |
| 201741046532-RELEVANT DOCUMENTS [15-07-2021(online)].pdf | 15/07/2021 |
| 201741046532-ABSTRACT [18-06-2021(online)].pdf | 18/06/2021 |
| 201741046532-CLAIMS [18-06-2021(online)].pdf | 18/06/2021 |
| 201741046532-DRAWING [18-06-2021(online)].pdf | 18/06/2021 |
| 201741046532-FER_SER_REPLY [18-06-2021(online)].pdf | 18/06/2021 |
| 201741046532-OTHERS [18-06-2021(online)].pdf | 18/06/2021 |
| 201741046532-ENDORSEMENT BY INVENTORS [18-12-2020(online)].pdf | 18/12/2020 |
| 201741046532-FORM 13 [31-03-2020(online)].pdf | 31/03/2020 |
| 201741046532-Amendment Of Application Before Grant - Form 13 [25-09-2018(online)].pdf | 25/09/2018 |
| 201741046532-ENDORSEMENT BY INVENTORS [25-09-2018(online)].pdf | 25/09/2018 |
| 201741046532-FORM 3 [13-09-2018(online)].pdf | 13/09/2018 |
| Form18_Normal Request_12-02-2018.pdf | 12/02/2018 |
| Description Complete_As Filed_26-12-2017.pdf | 26/12/2017 |
| Form1_As Filed_26-12-2017.pdf | 26/12/2017 |
| Form9_Earlier Publication_26-12-2017.pdf | 26/12/2017 |
Refer a friend