GAMMA PRIME PRECIPITATION STRENGTHENED NICKEL-BASE SUPERALLOY FOR USE IN POWDER BASED ADDITIVE MANUFACTURING PROCESS
Extensive patent search conducted by a registered patent agent
Patent search done by experts in under 48hrs
₹999
₹399
Abstract
Information
Inventors
Applicants
Specification
Documents
CONVENTIONAL APPLICATION
Published
Filed on 7 May 2015
Patent Information
| Application ID | 1272/DEL/2015 |
| Date of Application | 07/05/2015 |
Documents
| Name | Date |
|---|---|
| 1272-DEL-2015- Reply from DAE (18-08-2022).pdf | 18/08/2022 |
| 1272-DEL-2015-FER.pdf | 17/10/2021 |
| Letter to Atomic Energy-1272-DEL-2015.pdf | 17/10/2021 |
| 1272-DEL-2015-FORM 18 [08-05-2018(online)].pdf | 08/05/2018 |
| 1272-DEL-2015-FORM 3 [09-01-2018(online)].pdf | 09/01/2018 |
| Assignment [15-04-2017(online)].pdf | 15/04/2017 |
| Form 6 [15-04-2017(online)].pdf | 15/04/2017 |
| Power of Attorney [15-04-2017(online)].pdf | 15/04/2017 |
| 1272-DEL-2015-Correspondence-090117.pdf | 10/01/2017 |
| 1272-DEL-2015-OTHERS-090117.pdf | 10/01/2017 |
| 1272-DEL-2015-Power of Attorney-090117.pdf | 10/01/2017 |
| Form 13 [18-11-2016(online)].pdf | 18/11/2016 |
| Other Document [18-11-2016(online)].pdf | 18/11/2016 |
| Form 13 [10-11-2016(online)].pdf | 10/11/2016 |
| Other Document [10-11-2016(online)].pdf | 10/11/2016 |
| 1272-del-2015-Correspondence Others-(06-11-2015).pdf | 06/11/2015 |
| 1272-del-2015-Form-3-(06-11-2015).pdf | 06/11/2015 |
| 1272-del-2015-Correspondence Others-(19-08-2015).pdf | 19/08/2015 |
| 1272-del-2015-Form-1-(19-08-2015).pdf | 19/08/2015 |
| 1272-del-2015-Others-(19-08-2015).pdf | 19/08/2015 |
| 1272-del-2015-Correspondence Others-(07-05-2015).pdf | 07/05/2015 |
| 1272-del-2015-Form-1-(07-05-2015).pdf | 07/05/2015 |
| 1272-del-2015-Form-2-(07-05-2015).pdf | 07/05/2015 |
| 1272-del-2015-Form-3-(07-05-2015).pdf | 07/05/2015 |
| 1272-del-2015-Form-5-(07-05-2015).pdf | 07/05/2015 |
| 1272-del-2015-GPA-(07-05-2015).pdf | 07/05/2015 |
Refer a friend