A METHOD TO MAKE CNT/PT CATALYST WHEREIN THE SIZE OF THE PLATINUM NANO PARTICLES IS CONTROLLED USING MICROWAVE IRRADIATION

Patent Search in India

  • tick

    Extensive patent search conducted by a registered patent agent

  • tick

    Patent search done by experts in under 48hrs

₹999

₹399

Talk to expert

A METHOD TO MAKE CNT/PT CATALYST WHEREIN THE SIZE OF THE PLATINUM NANO PARTICLES IS CONTROLLED USING MICROWAVE IRRADIATION

ORDINARY APPLICATION

Published

date

Filed on 9 July 2015

Patent Information

Application ID746/KOL/2015
Date of Application09/07/2015

Documents

NameDate
746-KOL-2015-IntimationOfGrant07-02-2024.pdf07/02/2024
746-KOL-2015-PatentCertificate07-02-2024.pdf07/02/2024
746-KOL-2015-DRAWING [26-09-2019(online)].pdf26/09/2019
746-KOL-2015-FER_SER_REPLY [26-09-2019(online)].pdf26/09/2019
746-KOL-2015-FER.pdf28/03/2019
746-KOL-2015-(04-05-2016)-PETITION UNDER RULE 137.pdf04/05/2016
746-KOL-2015A-(04-05-2016)-CORRESPONDENCE.pdf04/05/2016
746-KOL-2015A-(04-05-2016)-FORM-1.pdf04/05/2016
Description(Complete) [03-05-2016(online)].pdf03/05/2016
Drawing [03-05-2016(online)].pdf03/05/2016
OTHERS [03-05-2016(online)].pdf03/05/2016
F2.pdf10/07/2015
F3.pdf10/07/2015
GPA.pdf10/07/2015
earn

Refer a friend